my profile |
register |
faq |
search upload photo | donate | calendar |
|
|
#21 |
|
Lifer
Lifetime Forum Patron Join Date: Dec 2003
Location: PORT ST LUCIE, FLORIDA
Posts: 12,216
Thanks: 6,209
Thanked 4,138 Times in 2,176 Posts
|
How did they avoid blueing the inside?????
|
|
|
|
|
|
#22 |
|
Lifer
Lifetime Forum Patron Join Date: Jul 2002
Location: VA
Posts: 3,592
Thanks: 1,773
Thanked 2,531 Times in 788 Posts
|
|
|
|
|
|
|
#23 |
|
Lifer
Lifetime Forum Patron Join Date: Dec 2003
Location: PORT ST LUCIE, FLORIDA
Posts: 12,216
Thanks: 6,209
Thanked 4,138 Times in 2,176 Posts
|
No relative of mine!
|
|
|
|
|
|
#24 |
|
User
Join Date: Jun 2002
Location: Byron, Georgia
Posts: 1,742
Thanks: 826
Thanked 1,788 Times in 590 Posts
|
The bluing was applied by hand; i.e., the whole part was not dipped in a solution. The rust bluing solution was wiped on and you may encounter a frame or part where a bit of the solution got on the area not intended to be blued. I've seen that on a Luger or two. Then the part is hung in a room to actually rust. The part was carded (wire brushed) to reveal the bluing underneath. The process was repeated until the depth of bluing desired was achieved.
Rust bluing is a beautiful finish but time and labor intensive. |
|
|
|
| The following member says Thank You to Doubs for your post: |
|
|
#25 |
|
Lifer
Lifetime Forum Patron Join Date: Dec 2003
Location: PORT ST LUCIE, FLORIDA
Posts: 12,216
Thanks: 6,209
Thanked 4,138 Times in 2,176 Posts
|
Thank You, Finally a logical explanation!!!!
|
|
|
|
![]() |
|
|