Hello all,
I recently purchased some guns from a widow. As I was finishing loading the gear, the lady said she found another pistol in the bathroom. Now, I had just bought $3k in various guns from her. I said O.K. I'm about spent out for the day I'll give you $200.00. Today I got around to looking at what I bought, it is a 41 -byf. The toggle, trigger, safety, mag release, take down lever and side plate have been nickel plated. The rest of the gun has been abrasive blasted (screwed huh?) inside and out. The good, all matching, even the grips, very tight and shoots great. Now, do I blue it, or Dura Coat for a shooter. TIA, for any help or comments. |
![]() |
![]() |
|
|