Default Rust Bluing on Welded/Soldiered Luger Parts

On the last Luger I rust blued when I stripped the old salt bluing from it, I found a place on the gun when a large pitted area was removed and filled in with welded metal. I worried that I got into a real problem and thought that it might have to be refinished in a Salt bluing (was this welding rod or silver soldier?)to cover this up! If it was soldier, then the salt bluing was out because of the highter temperature would melt the soldier. With some trepidation (is that a word?) I started the task of rust bluing! The gun came out fabulously and I was pleased to see I couldnt see the weld in the bluing pattern! WHEW! Was I pleased! ~Thor~



Thor is offline  
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 05:36 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com