Mike, In addition to the above, strawing of the small parts took less time and work than rust bluing those parts. When Mauser decided to hot dip the lugers and P38s for the military, as they had several years exoerience with the PP series et al, it made sense to also hot dip the small parts. TH
__________________
Tom Heller POB 398 ST.Charles, MO. 63302
Tel 636-447-3006 lugerdoc@charter.net
Lugerdoc is offline   Reply With Quote
The following 2 members says Thank You to Lugerdoc for your post:
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 02:34 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com