A 400 finish is fine for rust bluing....the rusting cycles are going to by their nature "matte" the finish a bit. My experience is the first cycle has the most effect on the final finish. It's hard to generalize, but say in a 80 degree 70% humidity environment, the first cycle should be about 4 hours I've found.
nukem556 is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:40 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com