While waiting for the C96 'test' piece to soak, I browsed the Web and found sites stating that Phosphoric acid would etch nickel/chrome...Various household products were mentioned...I don't have any of them...But Naval Jelly has Phosphoric acid in it (a very mild solution)...So I brushed that on one of the nickel plated Mec-Gar mags and left it overnight...The pic below shows how it affected the nickel...Not really etched...More like tarnished...

Not exactly what I'm looking for...But it is a step in the right direction...
Attached Images
File Type: jpg jelly_mags.jpg (55.0 KB, 125 views)
__________________
I like my coffee the
way I like my women...
...Cold and bitter...
sheepherder is offline  
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 04:57 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com