I'll see how its looking here in a few minutes but man I wish I knew about this 2 or 3 hour thing in the first place!
__________________
Trying to redo grand dads Luger the best I can.
Terry Tiell is offline   Reply With Quote
Unread 07-20-2012, 01:49 PM   #2
nukem556
User
 
nukem556's Avatar
 
Join Date: Jul 2010
Location: Irmo, SC
Posts: 625
Thanks: 35
Thanked 168 Times in 107 Posts
Default

Rusting time is very dependent on humidity levels too.....you might get away with a 6 hour first rust in the Mojave desert, but anywhere else, its too long. It's 95 degrees and 70% humidity here in SC today....if I did a 6 hour first rust cycle on bare metal today, there would be actual fine pitting all over it .
nukem556 is offline   Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 06:45 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com