![]() Quote:
No, I'd lay off using it until this issue is resolved. Anyway, Tig welding can fix it all the way through. I think it would be good to obtain an unserviceable part from a parts/donor Luger of the same period so that the filler metal for the work would be the same as your toggle link. I am ignorant about specific hardness the link should be, but since it is the same material, it can be annealed and heat treated again after the surface/shape/contour has been restored, but obviously before it is re-blued. Yes, Ted, let's see a pic of yours, for comparison. |
|
![]() |
![]() |
|
|