Olie,
Found it
http://www.caswellplating.com/kits/metalx.html
Thanks !!!
Bill
lfid is offline   Reply With Quote
Unread 10-03-2011, 03:11 PM   #2
Olle
User
 
Olle's Avatar
 
Join Date: Feb 2010
Location: Tennessee
Posts: 1,149
Thanks: 159
Thanked 664 Times in 318 Posts
Default

Quote:
Originally Posted by lfid View Post
Olie,
Found it
http://www.caswellplating.com/kits/metalx.html
Thanks !!!
Bill
Yep, B-9 is the one I use. The instructions say that you should heat it, but I get just as good results by degreasing thoroughly and leaving in cold solution overnight. Wire brush, rinse and repeat and that takes care of it. I know that some people are worried about etching, but I have never had a problem with that. As a matter of fact, when I stripped this one I found several areas that still looked plated so I soaked it again. It still wouldn't come off, but after wiping it with cold blue I realized that it was the polished steel under the nickel, still with a bright shine to it despite being soaked for two days. In other words: I'm not worried about etching at all.
Olle is offline   Reply With Quote
The following member says Thank You to Olle for your post:
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off