Default Re: After a closer look !

Judging by the quality of the welds and general design appearance, I'm forced to Change My Earlier Opinion to a WW-II product.

Spot welds show a lack of consistent pressure and electrical discharge control, resulting in shallow and deep spots with poor heat distribution over the spot area, and considerable spatter on some welds and some heat warping around welds.

In general the design speaks to me of Typical German WW-II Technology.

My Apology for an earlier Wrong Opinion!

ViggoG





 
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 07:53 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Lugerforum.com