Unread 04-23-2010, 10:48 AM   #3
alanint
User
 
alanint's Avatar
 
Join Date: Mar 2008
Location: Marco Island, Florida
Posts: 4,867
Thanks: 1,685
Thanked 1,917 Times in 1,193 Posts
Default

No. Nickel plating forms a non-porous surface that bluing will not react to. The plating must be stripped off before you can blue. Another possibility if stripping the nickel is not an option would be a coating such as gun kote. The downside would be the thickness of the coating on top of the nickel may affect certain tolerances. In those cases you would have to sand down the coating and hope the proper clearances are achieved.
alanint is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:16 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com