Howard,

Must be a lot more blue worn guns there than here. I'm going to start doing rust bluing as soon as my shop is complete. Don't need the hazards of salt bluing , but will probably do some now and then. I have all of Ron's salt bluing equipment.

He died of lung and liver cancer, suspected to be caused by inhaling the salts for all of those years. I have seen him come out of his shop with salt crystals hanging from his eyebrows and his glasses coated like frost.
__________________
I Still Need DWM side plate #49... if anyone runs across a nice one.


What ~Rudyard Kipling~ said...
Ron Smith is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:43 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com