Unread 04-15-2001, 06:07 PM   #14
Joe DeLong
Guest
 
Posts: n/a
Default Re: Strawing

Neil,


You do not need to heat the items selected for the straw more than once unless you are not happy with the color, and need to start over. Heat treatment is not a factor, as the parts are not exposed to much more than 300 degrees. The "quench" in light oil is intended to stop any color change the part might take on after removal from the heat source. The heat is "drawn" off rapidly, and the part will not take on any more color change. The oil is just a little slower than water, without worry of after-rust. In addition; you can improve the durability of the finish slightly by using a lower heat setting on the burner, allowing the part to reach color more slowly. Does take a little more patience tho. If you want any part "fire-blue"; increase the heat a little (around 600), and "cook" it longer. Don't do this to the take-down lever (locking bolt).



 
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:13 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com