David, in some of the images of nitrocarburized materials, the stuff looks pretty shiny. Melonite and Tenifer(?) finishes are used by a couple of manufacturers; my Glock has a flat/satin look to it. I've got no idea how it was prepared for finishing.
We still havent figured out why sodium nitrate and/or the other chemicals used in rust bluing impart a blue tone to iron oxide. At this point, I'm out of ideas.

John
Paladinpainter is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 11:51 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com