Old 07-20-2012, 08:43 AM   #8
Olle
User
 
Olle's Avatar
 
Join Date: Feb 2010
Location: Tennessee
Posts: 1,149
Thanks: 159
Thanked 664 Times in 318 Posts
Default

I just blued a Luger sideplate with Mark D's formula, and I got the same result as Terry. It blued quickly and easily, but ended up being the same "greasy black" as you get using Brownells formula straight out of the bottle.

One thing I noticed was that the modified formula was very thin. I usually heat the parts with a hairdryer and apply just enough formula to wet the surface. It will dry in a couple of seconds, and you will see a thin, dull coat of dried formula after the application. With this formula you could barely see that you had applied it, so maybe you need to use it in a "more aggressive" way, like applying several coats, using higher humidity etc? Mark's pictures of the rusting show a lot of red rust, but I didn't get any of that.
Olle is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 03:22 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com