Unread 07-01-2011, 11:21 PM   #1
nukem556
User
 
nukem556's Avatar
 
Join Date: Jul 2010
Location: Irmo, SC
Posts: 625
Thanks: 35
Thanked 168 Times in 107 Posts
Default Teaser....DWM blue!

Gallons of distilled water, nearly 30 different rust blue solutions and hours of slaving in a hot kitchen, I'm very close to what I consider a close match for the original DWM color. I began this Quixotian quest as a result of necessity, as there are restorers who will not share their formula, even though they have more work than they can get to. If the results meet my initial trials, I will gladly share the results with my fellow forum members.
The formula is very close to one documented here by an old member, "chuckc" (search old posts), with a couple of significant modifications. Sadly, he has stopped contributing or gone to his reward...a shame, as I'd loved to bounced ideas back and forth with him.
I'll be throwing my chips in the pot by using this mixture on an early 1900 Parabellum I bought in rough condition...hope to be able to share the results with you guys in about 3 weeks. Bob

Last edited by nukem556; 07-02-2011 at 11:54 AM.
nukem556 is offline   Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:04 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Lugerforum.com