Unread 01-14-2020, 04:42 PM   #1
DonVoigt
User
 
DonVoigt's Avatar
 
Join Date: Apr 2015
Location: near Charlotte NC
Posts: 4,681
Thanks: 1,443
Thanked 4,355 Times in 2,041 Posts
Default

De-rusted with phosphoric acid(naval jelly) = the color you describe.

Without pictures it didn't happen!
__________________
03man(Don Voigt); Luger student and collector.
Looking for DWM side plate: 69 ; Dreyse 1907 pistol K.S. Gendarmerie
DonVoigt is offline   Reply With Quote
Unread 01-14-2020, 06:40 PM   #2
G.T.
Lifer
Lifetime Forum
Patron
 
Join Date: Jun 2002
Location: Chandler Arizona
Posts: 3,530
Thanks: 1,334
Thanked 3,711 Times in 1,014 Posts
Default That's kind of up to the owner!

Hi Don, I felt that a full blown text would be at the discretion of the owner, as it was just submitted for repair and not really in my wheel house for publication... ... but, it was definitely plated, as it was the same on the layered parts inside the mainspring cup... It was the same zinc type of plating found on the .22 conversion box parts.... I agree, I should have taken pics, maybe I can talk the owner into doing so... best to you, til...lat'r.....GT....
G.T. is offline   Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 06:51 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Lugerforum.com