Default Re: Strawing

Dan, I agree with the 400 degrees and watching them carefully, as thinner parts will be done quicker than thicker ones. Also the polishing is important. If you want them to shine, you need a high polish, but to look original just use scotch bright or steel wool. Tom h.



 
 