Unread 08-20-2012, 01:34 PM   #22
command450
User
 
command450's Avatar
 
Join Date: Jun 2011
Location: West Michigan
Posts: 38
Thanks: 16
Thanked 6 Times in 4 Posts
Default

When I first seen this. I was just about to chime in and say, yes it can be saved. Ive done parkerizing and Bluing. I also have saved a few lugers,that would have been written off by many. park can be be removed easily with naval jelly,or other types of acids. all bluing proccess' are actually forms of rust. Nickle plating is a different story.

I personally think its by far the best route,to restore lugers when they have issues and this case its a shining example of why its worth doing!

Congrats to the O P.
command450 is offline   Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 11:48 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Lugerforum.com