Rusting time is very dependent on humidity levels too.....you might get away with a 6 hour first rust in the Mojave desert, but anywhere else, its too long. It's 95 degrees and 70% humidity here in SC today....if I did a 6 hour first rust cycle on bare metal today, there would be actual fine pitting all over it .
nukem556 is offline   Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:58 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com