I believe I would call it "heat treatment" or "drawing" or "tempering".
The colors range from light yellow through red and blue to grey. It can be done for decoration but is more often the result of drawing hardened parts to render them less brittle.

Fire blueing is a commonly used mis-nomer, there is a "fire" blue , sometimes called carbon bluing or carbonia bluing; I believe Colt was "famous" for this very pretty but not very durable blue.

Here are the colors and temperatures required to achieve them on polished steel. These are not "my" charts but borrowed from other posts on these forums.
Attached Thumbnails
Click image for larger version

Name:	Tempering_standards_used_in_blacksmithing.jpg
Views:	234
Size:	108.1 KB
ID:	70950  

Click image for larger version

Name:	home strawchart_1.sized.jpg
Views:	220
Size:	79.8 KB
ID:	70951  

__________________
03man(Don Voigt); Luger student and collector.
Looking for DWM side plate: 69 ; Dreyse 1907 pistol K.S. Gendarmerie
DonVoigt is offline   Reply With Quote
The following member says Thank You to DonVoigt for your post:
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 12:02 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Lugerforum.com