Brownells arrived. The 3.5% nickle steel rod after welding on base metal blues OK (rust blue). That's also a little bit surprise to me.

The pix shows how the trial bar looks after applying the oxidation agent the 2nd time (N times needed), not bad.... I mean it rusts not bad, my welding was horrible
Attached Thumbnails
Click image for larger version

Name:	Nickle Steel Filler.jpg
Views:	150
Size:	61.8 KB
ID:	10532  

alvin is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:02 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Lugerforum.com