A thought occurrred to me while reading this.

Some strawed parts--I'm thinking thumb safety particularly--are varying thicknesses. I wonder, if it would be useful to heat-soak parts to just below color formation in order to stabilize their temperature throughout, before cranking up to color temperature/time?