As far as duribility of gold goes it makes a big difference if it is plated with 22 or 24 K or say 14 K or 18 K or the best for durability would be 10 K. 10 K is much harder because of the metal alloys added to it. 24 K gold is similar to lead. Very bendable and soft. Lots of plating concernes plate in 22K and it is say , a car part or some such that is simply decorative without much wear involved. Pays to know what to ask for. Jerry Burney