Quote:
Originally Posted by Curss View Post
So thats where you get Kryptonite bullets.... If you don't mind me asking, whats the purpose of the Hi-Tek coating?
It's in essence a "jacket" that encapsulates the lead and renders bullet lube un needed. No lubing and no leading what so ever. Lubing 500 bulets on my Lyman 450 takes the best part of 2 hours, Hi-Tek coating tales less than 20min.

Oh and the colour actually is called kryptonite green
http://hi-performancebulletcoatings.com/

Last edited by Chickenthief; 02-27-2017 at 07:56 PM. Reason: Spelling errors