Quote:
Originally Posted by 4 Scale
The finish appears to have received moderate to heavy buffing and has been re-blued as evidenced by bluing over pitting. The grips are not original and appear to be Vopo (East German).
|
That ain't blueing over pitting. That's blueing over the heat damage done to the gun when the chamber was carelessly welded shut under the UKs brutal "Deactivation" program. In this case, with no regard to the pistols outer looks.
Within the confines of the UK laws, at least find an example that was treated with respect upon deactivation.