Thread: Rust Bluing
View Single Post
Unread 01-19-2011, 10:52 AM   #8
timn
User
 
Join Date: Jan 2011
Posts: 9
Thanks: 0
Thanked 1 Time in 1 Post
Exclamation

Originally Posted by hank678417
formula

nitric acid 4oz
hydrochloric acid 3oz
iron 1/2 lb
distilled water 1 quart

This is very close to the old Neidner formula.
Used correctly, you can get different "colorings" depending on the steel.

I refinished (again) my 1911 this way and it turned out exactly like I wanted.

CAUTION: Mixing these chemicals is dangerous.

AAA... Alway Add Acid to water.

When The iron (I used baling wire) is added to the acids it produces a very toxic gas. Do this outside with some breathing protection.