Default

Blueing is an oxidation process. Whether it is rust blueing or hot salt blueing, it results in an oxidized surface. Most blued guns turn reddish brown over time. Some quicker than others.
Deputywood is offline   Reply With Quote
The following 4 members says Thank You to Deputywood for your post:
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 12:18 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Lugerforum.com