The oldtimers made them springy by heating them in a bath of molten lead. It helped to get a uniform heat treatment at the right temperature.
The good old days without health code legislation
|
|
|
|
| The following 5 members says Thank You to Vlim for your post: |
|
|
#2 |
|
Lifer
Lifetime Forum Patron Join Date: Jun 2002
Location: Chandler Arizona
Posts: 3,550
Thanks: 1,361
Thanked 3,779 Times in 1,028 Posts
|
Hi Gerben, I have heard of the use of lead for drawing back spring that have been quenched, I use Nitre blue salts for the drawing process blue. Using formed annealed high carbon steel, 1075 or 1095, I first heat the part up with a torch to a bright orange and quench it in water. Some put a layer of oil on the water to reduce the shock, but I find water alone, at room temp, works fine. Once that is accomplished, I then polish the part totally with a fine Dremel buff and suspend it from a thin piece of wire. I have a small Lee lead pot that I use to bring the Nitre salts up to 600 degrees and I suspend the part with the wire bent over the edge to hold it true. I check every minute or so to see the color change and be Johnny on the spot when it reaches blue! It goes thru yellow, brown, violet, and light blue before it gets to blue, or even dark blue?I like purple and can't stand to go any further! I shine a small hign intensity flashlight on it to verify color. Once out of the pot and cooled, just use your thumbnail to remove and remaining salts that are still on the part, and wipe down with oil... That's it! You just made a spring! Best to all, til......lat'r.....GT...
![]()
|
|
|
|
| The following 3 members says Thank You to G.T. for your post: |
|
|
#3 |
|
Lifer
Lifetime Forum Patron Join Date: Jun 2002
Location: Chandler Arizona
Posts: 3,550
Thanks: 1,361
Thanked 3,779 Times in 1,028 Posts
|
Well, it's like rasing chickens, some make and some don't!
and so it is with the home made springs! One of them has survived several hundred cycles, and one just gave up the ghost shortly afer installation! So, do we give up? Not likely!I revisited the first attempt with the, "KING KONG!" springs that were too thick, but more importantly, a more forgiving alloy being SAE1075 more inline with shade tree attempts and results... I then thinned and tapered one of them to closely replicate the originals, and now have an understanding of why they go from thick to thin? I'm sending them off tomorrow, or there'abouts, and we will take another shot at this... best, til....lat'r....GT ![]()
|
|
|
|